With responsible good quality method, good status and excellent client services, the series of solutions produced by our company are exported to lots of countries and regions for Fiber Optic Patch Cord Factory, Fiber Optic Splice Closure Specification, Cost Of Fiber Optic Cable Per Meter, We warmly welcome you to establish cooperation and create a bright future together with us.
OEM/ODM Factory Blown Fiber Technology - Singlemode Fiber- G.652D Singlemode Fiber – Wasin Fujikura Detail:

Nanjing Wasin Fujikura G.652D Singlemode fiber, mainly used city network and access network. Prouduce according to supreme standard, performance excelled ITU-TGB/T9771 the newest standard.

performance

characteristic condition date unit
Optical specifications
Attenuation coefficient 1310nm1383nm1550nm1625nm <0.35≤0.34≤0.21≤0.24 dB/kmdB/kmdB/km dB/km
Attenuation vs.Wavelength @1310nm@1550nm 1285~1330nm1525~1575nm ≤0.04≤0.03 dB/kmdB/km
Wavelenth Dispersion 1285-1340nm1550nm1625nm ≥-3.5   ≤3.5≤18≤22 ps / (nm·km)ps / (nm·km)ps / (nm·km)
Zero-dispersion wavelength 1300~1324 nm
Zero-dispersion slope ≤0.092 ps/(nm2·km)
Polarization Mode Dispersion PMDSingle fiber maximal valueFiber link value (M=20Q=0.01%) ≤0.20≤0.10 ps/√kmps/√km
cable cuoff  wavelength ≤1260 nm
Mode field diameter MFD 1310nm 9.2±0.4 μm
Effective Group Index of Refraction Neff 1310nm1550nm 1.46751.4681
Point discontinuity 1550nm ≤0.05 dB
Dimensions performance
Cladding diameter 125±0.7 μm
Cladding  Non-circularity ≤0.5 %
Outer coating diameter 245±10 μm
Cladding/Coating Concentricity ≤12.0 μm
Core/cladding concentricity ≤0.5 μm
curvature (radius) ≥4 μm
length 2.0~50.4 km/reel
Environmental performance(1310nm/1550nm)
Damp heat 85℃, humidity≥85%, 30days ≤0.05 dB/km
Dry heat 85℃±2℃,30days ≤0.05 dB/km
Temperature Dependence -60℃ ~ +85℃, two weeks ≤0.05 dB/km
Water immersion 23℃±5C 30days ≤0.05 dB/km
Mechanical performance
Proof test level >0.69 GPa
Macrobend loss100 turnsφ60mm1 turnsφ32mm 1625nm1550nm ≤0.1≤0.05 dBdB
Strip force 1.0~5.0 N
Dynamic fatigue parameter ≥20

Product detail pictures:

OEM/ODM Factory Blown Fiber Technology - Singlemode Fiber- G.652D Singlemode Fiber – Wasin Fujikura detail pictures

OEM/ODM Factory Blown Fiber Technology - Singlemode Fiber- G.652D Singlemode Fiber – Wasin Fujikura detail pictures

OEM/ODM Factory Blown Fiber Technology - Singlemode Fiber- G.652D Singlemode Fiber – Wasin Fujikura detail pictures

OEM/ODM Factory Blown Fiber Technology - Singlemode Fiber- G.652D Singlemode Fiber – Wasin Fujikura detail pictures

OEM/ODM Factory Blown Fiber Technology - Singlemode Fiber- G.652D Singlemode Fiber – Wasin Fujikura detail pictures

OEM/ODM Factory Blown Fiber Technology - Singlemode Fiber- G.652D Singlemode Fiber – Wasin Fujikura detail pictures


Related Product Guide:

We constantly function like a tangible group to ensure that we can give you the very best high-quality and also the very best cost for OEM/ODM Factory Blown Fiber Technology - Singlemode Fiber- G.652D Singlemode Fiber – Wasin Fujikura , The product will supply to all over the world, such as: Croatia, Tunisia, Ukraine, Our company has always insisted on the business principle of "Quality, Honest, and Customer First" by which we have won the trust of clients both from at home and abroad. If you are interested in our products, please do not hesitate to contact us for further information.
  • Perfect services, quality products and competitive prices, we have work many times, every time is delighted, wish continue to maintain!
    5 Stars By Kim from Poland - 2017.11.01 17:04
    This enterprise in the industry is strong and competitive, advancing with the times and develop sustainable, we are very pleased to have a opportunity to cooperate!
    5 Stars By Miguel from Austria - 2018.07.26 16:51
    Write your message here and send it to us